General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 20.0 °C | 15 % Show Material materials with Elongation of 15 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 20.0 °C | 710 - 880 MPa Show Material materials with Tensile strength of 710 - 880 MPa | |
Yield strength | 20.0 °C | 580 - 620 MPa Show Material materials with Yield strength of 580 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 - 0.12 % Show Material materials with Carbon of 0.03 - 0.12 % |
Manganese | 0.3 - 1.8 % Show Material materials with Manganese of 0.3 - 1.8 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.