Steel 25CrMo4 is suitable for components with high strength and toughness requirements at mean and higher heat-treatment cross-sections in vehicle, engine and machine engineering (e.g. crankshafts, steering knuckles, pinions). Lowest working temperature -40 °C Further application for mounting elements at increased and lower temperatures.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.83 - 7.85 g/cm³

Show Material materials with Density of 7.83 - 7.85 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

-100.0 °C

217 GPa

Show Material materials with Elastic modulus of 217 GPa

20.0 °C

212 GPa

Show Material materials with Elastic modulus of 212 GPa

100.0 °C

205 - 207 GPa

Show Material materials with Elastic modulus of 205 - 207 GPa

200.0 °C

195 - 199 GPa

Show Material materials with Elastic modulus of 195 - 199 GPa

300.0 °C

185 - 192 GPa

Show Material materials with Elastic modulus of 185 - 192 GPa

400.0 °C

184 GPa

Show Material materials with Elastic modulus of 184 GPa

500.0 °C

175 GPa

Show Material materials with Elastic modulus of 175 GPa

600.0 °C

164 GPa

Show Material materials with Elastic modulus of 164 GPa

Elongation

20.0 °C

18 %

Show Material materials with Elongation of 18 %

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Chromium Molybdenum Steel

Reduction of area

20.0 °C

60 %

Show Material materials with Reduction of area of 60 %

Tensile strength

20.0 °C

600 - 750 MPa

Show Material materials with Tensile strength of 600 - 750 MPa

300.0 °C

460 MPa

Show Material materials with Tensile strength of 460 MPa

350.0 °C

440 MPa

Show Material materials with Tensile strength of 440 MPa

Unlock all property charts

Yield strength Rp0.2

20.0 °C

420 - 440 MPa

Show Material materials with Yield strength Rp0.2 of 420 - 440 MPa

50.0 °C

414 - 435 MPa

Show Material materials with Yield strength Rp0.2 of 414 - 435 MPa

100.0 °C

403 - 428 MPa

Show Material materials with Yield strength Rp0.2 of 403 - 428 MPa

150.0 °C

393 - 420 MPa

Show Material materials with Yield strength Rp0.2 of 393 - 420 MPa

200.0 °C

382 - 412 MPa

Show Material materials with Yield strength Rp0.2 of 382 - 412 MPa

250.0 °C

372 - 392 MPa

Show Material materials with Yield strength Rp0.2 of 372 - 392 MPa

300.0 °C

344 - 363 MPa

Show Material materials with Yield strength Rp0.2 of 344 - 363 MPa

350.0 °C

324 - 333 MPa

Show Material materials with Yield strength Rp0.2 of 324 - 333 MPa

400.0 °C

294 - 304 MPa

Show Material materials with Yield strength Rp0.2 of 294 - 304 MPa

450.0 °C

265 - 275 MPa

Show Material materials with Yield strength Rp0.2 of 265 - 275 MPa

500.0 °C

226 - 235 MPa

Show Material materials with Yield strength Rp0.2 of 226 - 235 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.05E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K

20.0 °C

1.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K

100.0 °C

1.11E-5 - 1.21E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.11E-5 - 1.21E-5 1/K

200.0 °C

1.21E-5 - 1.27E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.21E-5 - 1.27E-5 1/K

300.0 °C

1.29E-5 - 1.32E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.29E-5 - 1.32E-5 1/K

400.0 °C

1.35E-5 - 1.36E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.35E-5 - 1.36E-5 1/K

500.0 °C

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K

600.0 °C

1.44E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.44E-5 1/K

Unlock all property charts

Max service temperature, long

-40 - 200 °C

Show Material materials with Max service temperature, long of -40 - 200 °C

Melting point

1382 - 1529 °C

Show Material materials with Melting point of 1382 - 1529 °C

Typical for Chromium Molybdenum Steel

Specific heat capacity

-100.0 °C

423 J/(kg·K)

Show Material materials with Specific heat capacity of 423 J/(kg·K)

20.0 °C

461 J/(kg·K)

Show Material materials with Specific heat capacity of 461 J/(kg·K)

100.0 °C

479 J/(kg·K)

Show Material materials with Specific heat capacity of 479 J/(kg·K)

200.0 °C

499 J/(kg·K)

Show Material materials with Specific heat capacity of 499 J/(kg·K)

300.0 °C

517 J/(kg·K)

Show Material materials with Specific heat capacity of 517 J/(kg·K)

400.0 °C

536 J/(kg·K)

Show Material materials with Specific heat capacity of 536 J/(kg·K)

500.0 °C

558 J/(kg·K)

Show Material materials with Specific heat capacity of 558 J/(kg·K)

600.0 °C

587 J/(kg·K)

Show Material materials with Specific heat capacity of 587 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

41 W/(m·K)

Show Material materials with Thermal conductivity of 41 W/(m·K)

100.0 °C

11.1 - 42.7 W/(m·K)

Show Material materials with Thermal conductivity of 11.1 - 42.7 W/(m·K)

200.0 °C

12.1 - 42.8 W/(m·K)

Show Material materials with Thermal conductivity of 12.1 - 42.8 W/(m·K)

300.0 °C

12.9 - 41.6 W/(m·K)

Show Material materials with Thermal conductivity of 12.9 - 41.6 W/(m·K)

400.0 °C

39.9 W/(m·K)

Show Material materials with Thermal conductivity of 39.9 W/(m·K)

500.0 °C

37.8 W/(m·K)

Show Material materials with Thermal conductivity of 37.8 W/(m·K)

600.0 °C

35.6 W/(m·K)

Show Material materials with Thermal conductivity of 35.6 W/(m·K)

Unlock all property charts

Thermal diffusivity

20.0 °C

11.4 mm²/s

Show Material materials with Thermal diffusivity of 11.4 mm²/s

100.0 °C

11 mm²/s

Show Material materials with Thermal diffusivity of 11 mm²/s

200.0 °C

10.3 mm²/s

Show Material materials with Thermal diffusivity of 10.3 mm²/s

300.0 °C

9.5 mm²/s

Show Material materials with Thermal diffusivity of 9.5 mm²/s

400.0 °C

8.5 mm²/s

Show Material materials with Thermal diffusivity of 8.5 mm²/s

500.0 °C

7.3 mm²/s

Show Material materials with Thermal diffusivity of 7.3 mm²/s

600.0 °C

6 mm²/s

Show Material materials with Thermal diffusivity of 6 mm²/s

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

2.54E-7 Ω·m

Show Material materials with Electrical resistivity of 2.54E-7 Ω·m

100.0 °C

3E-7 Ω·m

Show Material materials with Electrical resistivity of 3E-7 Ω·m

200.0 °C

3.69E-7 Ω·m

Show Material materials with Electrical resistivity of 3.69E-7 Ω·m

300.0 °C

4.51E-7 Ω·m

Show Material materials with Electrical resistivity of 4.51E-7 Ω·m

400.0 °C

5.45E-7 Ω·m

Show Material materials with Electrical resistivity of 5.45E-7 Ω·m

500.0 °C

6.54E-7 Ω·m

Show Material materials with Electrical resistivity of 6.54E-7 Ω·m

600.0 °C

7.78E-7 Ω·m

Show Material materials with Electrical resistivity of 7.78E-7 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Carbon

0.22 - 0.29 %

Show Material materials with Carbon of 0.22 - 0.29 %

Chromium

0.9 - 1.2 %

Show Material materials with Chromium of 0.9 - 1.2 %

Manganese

0.6 - 0.9 %

Show Material materials with Manganese of 0.6 - 0.9 %

Molybdenum

0.15 - 0.3 %

Show Material materials with Molybdenum of 0.15 - 0.3 %

Phosphorus

0.03 - 0.04 %

Show Material materials with Phosphorus of 0.03 - 0.04 %

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Sulfur

0.035 %