Primary standard name

Properties

Mechanical

Hardness, Brinell HB

0 - 95 [-] at 20 °C

Tensile strength Rm

310 MPa at 20 °C

Yield strength YS

0 - 276 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Al

95.8 - 98.61 %

Mg

0.8 - 1.2 %

Si

0.4 - 0.8 %

Cu

0.15 - 0.4 %

Cr

0.04 - 0.35 %

More

Technological properties

Processing history

T651