General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Hardness, Brinell | 23.0 °C | 90 - 204 [-] Show Material materials with Hardness, Brinell of 90 - 204 [-] | |
Hardness, Rockwell B | 23.0 °C | 50 - 99 [-] Show Material materials with Hardness, Rockwell B of 50 - 99 [-] | |
Hardness, Rockwell C | 23.0 °C | 21 [-] Show Material materials with Hardness, Rockwell C of 21 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Tensile strength | 23.0 °C | 340 - 740 MPa Show Material materials with Tensile strength of 340 - 740 MPa |