JIS G4315 Grade SUS384-WSB

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

20 - 25 %

Show Material materials with Elongation A5 of 20 - 25 %

Reduction of area

20.0 °C

65 %

Show Material materials with Reduction of area of 65 %

Tensile strength

20.0 °C

460 - 690 MPa

Show Material materials with Tensile strength of 460 - 690 MPa

Chemical properties

PropertyValue

Carbon

0.08 %

Show Material materials with Carbon of 0.08 %

Chromium

15 - 17 %

Show Material materials with Chromium of 15 - 17 %

Iron

60.84 - 68 %

Show Material materials with Iron of 60.84 - 68 %

Manganese

2 %

Show Material materials with Manganese of 2 %

Nickel

17 - 19 %

Show Material materials with Nickel of 17 - 19 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %