Mechanical

PropertyTemperatureValue

Elongation A5

23.0 °C

5 %

Show Material materials with Elongation A5 of 5 %

Hardness, Brinell

23.0 °C

163 [-]

Show Material materials with Hardness, Brinell of 163 [-]

Tensile strength

23.0 °C

270 MPa

Show Material materials with Tensile strength of 270 MPa

Yield strength Rp0.2

23.0 °C

165 MPa