JIS C2555 Grade PCYC300-TF182 cold-rolled

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A80

20.0 °C

15 %

Show Material materials with Elongation A80 of 15 %

Tensile strength

20.0 °C

375 MPa

Show Material materials with Tensile strength of 375 MPa

Yield strength Rp0.2

20.0 °C

300 MPa

Show Material materials with Yield strength Rp0.2 of 300 MPa

Technological properties

Property
Processing history

cold-rolled