JIS C2555 Grade PCYH600-TG178 hot-rolled

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A5

20.0 °C

12 %

Show Material materials with Elongation A5 of 12 %

Elongation A80

20.0 °C

10 %

Show Material materials with Elongation A80 of 10 %

Tensile strength

20.0 °C

700 MPa

Show Material materials with Tensile strength of 700 MPa

Yield strength Rp0.2

20.0 °C

600 MPa

Show Material materials with Yield strength Rp0.2 of 600 MPa

Technological properties

Property
Processing history

hot-rolled