Description

Primary standard name

Properties

Mechanical

Reduction of area Z

30 - 45 % at 20 °C

Tensile strength Rm

1530 - 2260 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

96.13 - 97.09 %

Si

1.2 - 1.6 %

Mn

0.6 - 0.8 %

Cr

0.6 - 0.8 %

C

0.51 - 0.59 %

More

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.