ASTM A485 Grade 4 coils hot-rolled, annealed

.XLSX
.PDF
Save

Description

Primary standard name

Equivalent standard names

Properties

Mechanical

Hardness, Rockwell B HRB

97 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

94.45 - 96.3 %

Cr

1.1 - 1.5 %

Mn

1.05 - 1.35 %

C

0.95 - 1.1 %

Mo

0.45 - 0.6 %

More

Technological properties

Processing history

coils

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.