ASTM A678 Grade A Quenched and Tempered

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

22 % at 20 °C

Tensile strength Rm

485 - 620 MPa at 20 °C

Yield strength YS

345 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.9 - 1.5 %

Cr

0.25 %

Ni

0.25 %

Cu

0.2 - 0.35 %

C

0.16 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.