ASTM A328 Grade

Get more information
Contact Matmatch

Standards

Properties

Mechanical

Tensile strength [ Rm ]

485.00 MPa

Yield strength [ YS ]

270.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software