ASTM A333 Grade 10

Get more information
Contact Matmatch

Standards

Chemical composition

Element Weight %
Fe 97.0699 — 98.7499
Mn 1.15 — 1.5
Si 0.1 — 0.35
Ni 0.0 — 0.25
C 0.0 — 0.2
Cr 0.0 — 0.15
Cu 0.0 — 0.15
V 0.0 — 0.12
Al 0.0 — 0.06
Nb 0.0 — 0.05
Mo 0.0 — 0.05
P 0.0 — 0.035
S 0.0 — 0.015

Properties

Mechanical

Tensile strength

[ Rm ]

Tensile strength

0—550.00 MPa

Yield strength

[ YS ]

Yield strength

0—450.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.