ASTM A336 Grade F3VCb

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Reduction of area Z

45 % at 20 °C

Tensile strength Rm

0 - 760 MPa at 20 °C

Yield strength YS

415 MPa at 20 °C