General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 23.0 °C | 40 % Show Material materials with Reduction of area of 40 % | |
Tensile strength | 23.0 °C | 620 - 830 MPa Show Material materials with Tensile strength of 620 - 830 MPa | |
Yield strength | 23.0 °C | 440 MPa Show Material materials with Yield strength of 440 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Boron | 3E-4 - 6E-3 % Show Material materials with Boron of 3E-4 - 6E-3 % |
Carbon | 0.09 - 0.13 % Show Material materials with Carbon of 0.09 - 0.13 % |
Chromium | 8.5 - 9.5 % Show Material materials with Chromium of 8.5 - 9.5 % |
Manganese | 0.3 - 0.6 % Show Material materials with Manganese of 0.3 - 0.6 % |
Molybdenum | 0.9 - 1.1 % Show Material materials with Molybdenum of 0.9 - 1.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.06 - 0.1 % Show Material materials with Niobium of 0.06 - 0.1 % |
Nitrogen | 0.04 - 0.09 % Show Material materials with Nitrogen of 0.04 - 0.09 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.1 - 0.5 % Show Material materials with Silicon of 0.1 - 0.5 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |
Titanium | 0.01 % Show Material materials with Titanium of 0.01 % |
Tungsten | 0.9 - 1.1 % Show Material materials with Tungsten of 0.9 - 1.1 % |
Vanadium | 0.18 - 0.25 % Show Material materials with Vanadium of 0.18 - 0.25 % |
Zirconium | 0.01 % Show Material materials with Zirconium of 0.01 % |