ASTM A354 Grade BC

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Hardness, Brinell HB

235 - 331 [-] at 20 °C

Hardness, Rockwell C HRC

22 - 36 [-] at 20 °C

Reduction of area Z

0 - 50 % at 20 °C

Tensile strength Rm

0 - 862 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

99.36 - 99.72 %

C

0.3 - 0.55 %

S

0 - 0.05 %

P

0 - 0.35 %

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.