Search for materials or suppliers
matmatch.com/materials/MINFM51215

ASTM A354 Grade BD

Get more information
Contact Matmatch

Standards

Chemical composition

Element Weight %
Fe 99.3649 — 99.6699
C 0.35 — 0.55
P 0.0 — 0.35
S 0.0 — 0.045

Properties

Mechanical

Hardness, Brinell [ HB ]

293.00—363.00 [-]

Hardness, Rockwell C [ HRC ]

31.00—39.00 [-]

Reduction of area [ Z ]

40.00 %

Tensile strength [ Rm ]

0—1034 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Download material data

Material data to download as .xlsx and .pdf file.