Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy | 23.0 °C | 18 J Show Material materials with Charpy impact energy of 18 J |
Elongation A50 | 23.0 °C | 28 % Show Material materials with Elongation A50 of 28 % |
Tensile strength | 23.0 °C | 435 MPa Show Material materials with Tensile strength of 435 MPa |
Yield strength | 23.0 °C | 315 MPa Show Material materials with Yield strength of 315 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.2 % Show Material materials with Carbon of 0.2 % |
Copper | 0.75 - 1.25 % Show Material materials with Copper of 0.75 - 1.25 % |
Manganese | 0.4 - 1.06 % Show Material materials with Manganese of 0.4 - 1.06 % |
Nickel | 1.6 - 2.24 % Show Material materials with Nickel of 1.6 - 2.24 % |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |