ASTM A405 Grade P24 heat treated

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Tensile strength Rm

0 - 350 MPa at 20 °C

Yield strength YS

0 - 345 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

96.22 - 97.78 %

Mo

0.87 - 1.13 %

Cr

0.8 - 1.25 %

Mn

0.3 - 0.6 %

V

0.15 - 0.25 %

More

Technological properties

Processing history

heat treated

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.