Tensile strength Rm
415 MPa at 20 °C
Yield strength YS
255 MPa at 20 °C
Element
Weight %
Comment
96.37 - 99.3 %
0.24 - 1.31 %
0.2 - 0.7 %
0.2 - 0.6 %
0.06 - 0.16 %
This material data has been provided by MetalInfo.