Reduction of area Z
50 % at 20 °C
Tensile strength Rm
485 MPa at 20 °C
Yield strength YS
205 MPa at 20 °C
Element
Weight %
Comment
69.08 - 76.45 %
14.5 - 16.5 %
7.5 - 9.5 %
1.5 - 2 %
0.05 - 0.1 %