ASTM A27 Grade 60-30 Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Show Material materials with Density of 7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Show Material materials with Elastic modulus of 200 - 215 GPa

Typical for Low Carbon Steel

Elongation A50

20.0 °C

24 %

Show Material materials with Elongation A50 of 24 %

Poisson's ratio

20.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Low Carbon Steel

Reduction of area

20.0 °C

35 %

Show Material materials with Reduction of area of 35 %

Shear modulus

20.0 °C

75 - 80 GPa

Show Material materials with Shear modulus of 75 - 80 GPa

Typical for Carbon Steel

Tensile strength

20.0 °C

415 MPa

Show Material materials with Tensile strength of 415 MPa

Yield strength

20.0 °C

205 MPa

Show Material materials with Yield strength of 205 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 - 1.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1480 - 1526 °C

Show Material materials with Melting point of 1480 - 1526 °C

Typical for Low Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

20.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Magnetic

PropertyTemperatureValueComment

Curie temperature

20.0 °C

770 °C

Show Material materials with Curie temperature of 770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

0.3 %

Show Material materials with Carbon of 0.3 %

Manganese

0.6 %

Show Material materials with Manganese of 0.6 %

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

Sulfur

0.035 %

Show Material materials with Sulfur of 0.035 %