ASTM A389 Grade C24

Get more information
Contact Matmatch

Equivalent standards

Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 95.6149 — 97.8499
Cr 0.8 — 1.25
Mo 0.9 — 1.2
Mn 0.3 — 0.8
Si 0.0 — 0.6
V 0.15 — 0.25
C 0.0 — 0.2
S 0.0 — 0.045
P 0.0 — 0.04

Properties

Mechanical

Reduction of area [ Z ]

35.00 %

Tensile strength [ Rm ]

552.00 MPa

Yield strength [ YS ]

345.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM53050 to find materials similar to ASTM A389 Grade C24.