ASTM A395 Grade F32800

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Hardness, Brinell HB

0 - 187 [-] at 20 °C

Tensile strength Rm

415 MPa at 20 °C

Yield strength YS

275 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Si

0 - 2.5 %

P

0 - 0.08 %

C

0 - 3 %

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.