Hardness, Brinell HB
0 - 248 [-] at 20 °C
Tensile strength Rm
207 MPa at 20 °C
Element
Weight %
Comment
64.08 - 77.5 %
18 - 22 %
3 - 6 %
1 - 2.8 %
0.5 - 1.5 %
This material data has been provided by MetalInfo.