Customize your search with filters
Do you have any questions?
Hardness, Brinell HB
0 - 159 [-] at 20 °C
Tensile strength Rm
172 MPa at 20 °C
Element
Weight %
Comment
57.78 - 68 %
28 - 32 %
2.5 - 3.5 %
1 - 2 %
0.5 - 1.5 %
This material data has been provided by MetalInfo.