Property | Value |
---|---|
Carbon | 2 - 3.3 % Show Material materials with Carbon of 2 - 3.3 % |
Chromium | 11 - 14 % Show Material materials with Chromium of 11 - 14 % |
Copper | 1.2 % Show Material materials with Copper of 1.2 % |
Manganese | 2 % Show Material materials with Manganese of 2 % |
Molybdenum | 3 % Show Material materials with Molybdenum of 3 % |
Nickel | 2.5 % Show Material materials with Nickel of 2.5 % |
Phosphorus | 0.1 % Show Material materials with Phosphorus of 0.1 % |
Silicon | 1.5 % Show Material materials with Silicon of 1.5 % |
Sulfur | 0.06 % Show Material materials with Sulfur of 0.06 % |