General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 7.9 - 8.2 g/cm³ Show Material materials with Density of 7.9 - 8.2 g/cm³ at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 195 GPa Show Material materials with Elastic modulus of 195 GPa at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Shear modulus | 77 GPa Show Material materials with Shear modulus of 77 GPa at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Tensile strength | 585 - 860 MPa Show Material materials with Tensile strength of 585 - 860 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 1.9E-5 1/K at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Melting point | 1230 - 1480 °C Show Material materials with Melting point of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 440 J/(kg·K) Show Material materials with Specific heat capacity of 440 J/(kg·K) at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Thermal conductivity | 11 - 21 W/(m·K) Show Material materials with Thermal conductivity of 11 - 21 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Electrical resistivity | 8.5E-7 Ω·m Show Material materials with Electrical resistivity of 8.5E-7 Ω·m at 23.0 °C | 23.0 °C | Typical for Austenitic Stainless Steel |
Chemical properties
Property | ||
---|---|---|
Carbon | 0.15 % | |
Chromium | 17 - 19 % | |
Manganese | 2 % | |
Nickel | 8 - 10 % | |
Phosphorus | 0.2 % | |
Silicon | 1 % | |
Sulfur | 0.06 % |