Mechanical

PropertyTemperatureValue

Elongation A200

23.0 °C

17 %

Show Material materials with Elongation A200 of 17 %

Elongation A50

23.0 °C

20 %

Show Material materials with Elongation A50 of 20 %

Tensile strength

23.0 °C

550 - 690 MPa

Show Material materials with Tensile strength of 550 - 690 MPa

Yield strength

23.0 °C

345 MPa

Show Material materials with Yield strength of 345 MPa

Chemical properties

PropertyValue

Carbon

0.2 %

Show Material materials with Carbon of 0.2 %

Manganese

1.15 - 1.5 %

Show Material materials with Manganese of 1.15 - 1.5 %

Molybdenum

0.45 - 0.6 %

Show Material materials with Molybdenum of 0.45 - 0.6 %

Nickel

0.4 - 0.7 %

Show Material materials with Nickel of 0.4 - 0.7 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.4 %

Show Material materials with Silicon of 0.15 - 0.4 %

Sulfur

0.025 %