Chemical composition

Element Weight %
Fe 98.1099 — 99.2499
Mn 0.6 — 0.9
C 0.0 — 0.55
Si 0.15 — 0.35
S 0.0 — 0.05
P 0.0 — 0.04

Properties

Mechanical

Reduction of area [ Z ]

35.00—45.00 %

Tensile strength [ Rm ]

590.00—760.00 MPa

Yield strength [ YS ]

345.00—520.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Download material data

Material data to download as .xlsx and .pdf file.

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM54715 to find materials similar to ASTM A321 Grade K05501.