Chemical composition

Element Weight %
Fe 61.8249 — 71.9599
Cr 16.0 — 18.0
Ni 10.0 — 14.0
Mo 2.0 — 3.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
C 0.04 — 0.1
P 0.0 — 0.045
S 0.0 — 0.03

Properties

Mechanical

Reduction of area [ Z ]

45.00 %

Tensile strength [ Rm ]

485.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A336 Grade F316H:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM54743 to find materials similar to ASTM A336 Grade F316H.