ASTM A336 Grade F316LN

Get more information
Contact Matmatch

Equivalent standards

GB/T 1220 Grade 00Cr17Ni13Mo2N GB/T 3280 Grade 00Cr17Ni13Mo2N GB/T 4237 Grade 00Cr17Ni13Mo2N GB/T 6967 Grade ZG10Cr13 More GB 4239 Grade 00Cr17Ni13Mo2N DIN 1654-5 Grade X2CrNiMoN17133 DIN 17440 Grade X2CrNiMoN17122 DIN 17440 Grade X2CrNiMoN17133 DIN 17441 Grade X2CrNiMoN17122 DIN 17441 Grade X2CrNiMoN17133 DIN 17455 Grade X2CrNiMoN17133 DIN 17456 Grade X2CrNiMoN17133 DIN 17457 Grade X2CrNiMoN17133 DIN 17458 Grade X2CrNiMoN17133 EN 10028-7 Grade X2CrNiMoN17-11-2 EURONORM 88-1 Grade X2CrNiMoN17122 EURONORM 88-2 Grade X2CrNiMoN17122 EURONORM 88-3 Grade X2CrNiMoN17122 SFS 753 Grade X2CrNiMoN17113 NF A35-582 Grade Z2CND17-12Az NF A35-582 Grade Z2CND17-13Az NF A35-573 Grade Z3CND17-11Az NF A35-573 Grade Z3CND17-12Az NF A36-209 Grade Z3CND17-11Az NF A36-209 Grade Z3CND17-12Az BS Grade 1501-3 BS Grade 1502 BS Grade 1506 ISO 4954 Grade X2CrNiMoN17133E ISO 2604-4 Grade X2CrNiMoN1712 ISO 2604-4 Grade X2CrNiMoN1713 UNI 7500 Grade X2CrNiMoN1712 UNI 7500 Grade X2CrNiMoN1713 UNI 8317 Grade X2CrNiMoN1713 UNI 8317 Grade X2CrNiMoN1712 ÖNORM M3121 Grade X2CrNiMoN17122KKW ÖNORM M3121 Grade X2CrNiMoN17133KKW EN 10088-1 Grade X2CrNiMoN17-11-2 EN 10088-2 Grade X2CrNiMoN17-11-2 EN 10088-3 Grade X2CrNiMoN17-11-2 EN 10222-5 Grade X2CrNiMoN17-11-2 EN 10272 Grade X2CrNiMoN17-11-2 UNE 36017 Grade X8CrNiMo27-05 UNE 36016-1 Grade X2CrNiMoN17122 UNE 36016-1 Grade X2CrNiMoN17133 UNE 36016-2 Grade X2CrNiMoN17122 UNE 36016-2 Grade X2CrNiMoN17133 UNE 36087 Grade X2CrNiMoN17122 UNE 36087 Grade X2CrNiMoN17133 SIS 142375 Grade 2375 ASTM A213 Grade TP316LN ASTM A269 Grade TP316LN ASTM A276 Grade 316LN ASTM A312 Grade TP316LN ASTM A320 Grade B8MLN ASTM A320 Grade B8MLNA ASTM A403 Grade CR316LN ASTM A403 Grade WP316LN ASTM A943 Grade TP316LN ASTM A959 Grade 316LN ASTM A988 Grade 18Cr ASTM A965 Grade F316LN ASTM A182 Grade F316LN ASTM A194 Grade 8MLN ASTM A249 Grade TP316LN ASTM A376 Grade TP316LN ASTM A688 Grade TP316LN ASTM A813 Grade TP316LN ASTM A814 Grade TP316LN ASTM A193 Grade B8MLN ASTM A167 Grade 316LN ASTM A240 Grade 316LN ASTM A479 Grade 316LN ASTM A193 Grade B8MLNA ASTM A194 Grade 8MLNA UNS Grade S31653 JIS G4306 Grade SUS316LN JIS G4307 Grade SUS316LN JIS G4303 Grade SUS316LN JIS G4304 Grade SUS316LN JIS G4305 Grade SUS316LN AISI 316LN ISO 9328-5 Grade X2CrNiMoN1712 ISO TR Grade 15510 EN 10250-4 Grade X2CrNiMoN17-11-2 SAE J405 Grade 316LN EN 10028-7 Grade X2CrNiMoN17-13-3 EN 10088-1 Grade X2CrNiMoN17-13-3 EN 10088-2 Grade X2CrNiMoN17-13-3 EN 10088-3 Grade X2CrNiMoN17-13-3 EN 10216-5 Grade X2CrNiMoN17-13-3 EN 10217-7 Grade X2CrNiMoN17-13-3 EN 10222-5 Grade X2CrNiMoN17-13-3 EN 10272 Grade X2CrNiMoN17-13-3 EN 10269 Grade X2CrNiMoN17-13-3 ASTM A336 Grade F316LN ISO 9328-5 Grade X2CrNiMoN1713 ISO 9330-6 Grade X2CrNiMoN1713 ISO 9329-4 Grade X2CrNiMoN1713 EN 10250-4 Grade X2CrNiMoN17-13-3
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Chemical composition

Element Weight %
Fe 61.7399 — 71.8999
Cr 16.0 — 18.0
Ni 10.0 — 14.0
Mo 2.0 — 3.0
Mn 0.0 — 2.0
Si 0.0 — 1.0
N 0.1 — 0.16
P 0.0 — 0.04
C 0.0 — 0.03
S 0.0 — 0.03

Properties

Mechanical

Reduction of area [ Z ]

45.00 %

Tensile strength [ Rm ]

485.00 MPa

Yield strength [ YS ]

205.00 MPa

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A336 Grade F316LN:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM54746 to find materials similar to ASTM A336 Grade F316LN.