ASTM A355 Grade A Range 1

Get more information
Contact Matmatch

Standards

Chemical composition

Element Weight %
Fe 94.9449 — 96.3199
Cr 1.4 — 1.8
Al 0.95 — 1.3
Mn 0.5 — 0.7
C 0.38 — 0.43
Mo 0.3 — 0.4
Si 0.15 — 0.35
S 0.0 — 0.04
P 0.0 — 0.035

Properties

Mechanical

Hardness, Brinell [ HB ]

0—289.00 [-]

Hardness, Rockwell B [ HRB ]

0—104.00 [-]

Hardness, Rockwell C [ HRC ]

0—28.00 [-]

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.

Technological properties

Processing history
Range 1
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software

Suppliers of Steel

The following suppliers might provide ASTM A355 Grade A Range 1:

Similar Materials

These are materials almost identical to the ones you are looking at. They could be a relevant standard or a different supplier.

Go to matmatch.com/materials/MINFM54756 to find materials similar to ASTM A355 Grade A Range 1.