Hardness, Brinell HB
0 - 302 [-] at 20 °C
Hardness, Rockwell B HRB
0 - 107 [-] at 20 °C
Hardness, Rockwell C HRC
0 - 32 [-] at 20 °C
Element
Weight %
Comment
94.9 - 96.35 %
1.2 - 1.5 %
0.95 - 1.3 %
0.7 - 0.95 %
0.35 - 0.4 %
Processing history
Range 2
This material data has been provided by MetalInfo.