Chemical composition

Element Weight %
Fe 91.9049 — 93.7299
Ni 3.25 — 3.75
Cr 1.0 — 1.35
Al 0.95 — 1.3
Mn 0.5 — 0.7
Si 0.15 — 0.35
Mo 0.2 — 0.3
C 0.22 — 0.27
S 0.0 — 0.04
P 0.0 — 0.035

Properties

Mechanical

Hardness, Brinell

[ HB ]

Hardness, Brinell

0—302.00 [-]

Hardness, Rockwell B

[ HRB ]

Hardness, Rockwell B

0—107.00 [-]

Hardness, Rockwell C

[ HRC ]

Hardness, Rockwell C

0—32.00 [-]

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.

Technological properties

Processing history
Range 2
Metalinfo, Eagle International Software
This material data has been provided by Metalinfo, Eagle International Software
Go to matmatch.com/materials/MINFM54761 to find materials similar to ASTM A355 Grade C Range 2.