ASTM A355 Grade D Range 1

.XLSX
.PDF
Save

Description

Properties

Mechanical

Hardness, Brinell HB

0 - 289 [-] at 20 °C

Hardness, Rockwell B HRB

0 - 104 [-] at 20 °C

Hardness, Rockwell C HRC

0 - 28 [-] at 20 °C

Chemical properties

Element

Weight %

Comment

Fe

95.64 - 96.92 %

Cr

1 - 1.3 %

Al

0.95 - 1.3 %

Mn

0.5 - 0.7 %

C

0.33 - 0.38 %

More

Technological properties

Processing history

Range 1

This material data has been provided by MetalInfo.