Customize your search with filters
Do you have any questions?
Reduction of area Z
50 % at 20 °C
Tensile strength Rm
600 MPa at 20 °C
Yield strength YS
310 MPa at 20 °C
Element
Weight %
Comment
62.63 - 68.43 %
20 - 22 %
10 - 12 %
1.4 - 2 %
0.14 - 0.2 %
This material data has been provided by MetalInfo.