ASTM A668 Class EH Normalized and tempered or double-normalized and tempered

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A50 A50

22 - 25 % at 20 °C

Hardness, Brinell HB

174 - 217 [-] at 20 °C

Reduction of area Z

35 - 40 % at 20 °C

Tensile strength Rm

570 - 585 MPa at 20 °C

Yield strength YS

295 - 305 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1.35 %

P

0.05 %

S

0.03 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.