ASTM A668 Class FH Quenched and tempered, or normalized, quenched and tempered

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A50 A50

19 - 20 % at 20 °C

Hardness, Brinell HB

174 - 235 [-] at 20 °C

Reduction of area Z

36 - 39 % at 20 °C

Tensile strength Rm

565 - 620 MPa at 20 °C

Yield strength YS

330 - 380 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1.35 %

P

0.05 %

S

0.03 %