Mechanical

Elongation A50 A50

12 - 15 % at 20 °C

Hardness, Brinell HB

269 - 352 [-] at 20 °C

Reduction of area Z

38 - 45 % at 20 °C

Tensile strength Rm

930 - 1000 MPa at 20 °C

Yield strength YS

758 - 825 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

P

0.04 %

S

0.03 %