Mechanical

Elongation A50

A50

11 - 13 % at 20 °C

Hardness, Brinell

HB

321 - 402 [-] at 20 °C

Reduction of area

Z

35 - 40 % at 20 °C

Tensile strength

Rm

1100 - 1175 MPa at 20 °C

Yield strength

YS

900 - 965 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

P

0.04 %

S

0.025 %