This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Hardness, Brinell HB
0 - 241 [-] at 20 °C
Melting point Tm
1370 - 1425 °C
Typical for Tool And Machining Steel
Specific heat capacity cp
420 - 460 J/(kg·K) at 20 °C
Typical for Tool And Machining Steel
Thermal conductivity λ
17 - 42 W/(m·K) at 20 °C
Typical for Tool And Machining Steel
Element
Weight %
Comment
14 - 16 %
2.5 - 3.5 %
0.42 - 0.53 %
0.4 - 0.6 %
0.15 - 0.4 %
This material data has been provided by ASTM.