ASTM A823 Grade A-SB Uncored-Annealed

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Hardness, Brinell HB

163 - 207 [-] at 20 °C

Tensile strength Rm

172 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

C

3.3 - 3.7 %

Si

2.2 - 2.8 %

P

0.45 %

Mn

0.4 - 1 %

S

0.15 %