Hardness, Brinell HB
170 - 229 [-] at 20 °C
Tensile strength Rm
0 - 207 MPa at 20 °C
Element
Weight %
Comment
3.3 - 3.7 %
2.2 - 2.8 %
0.4 - 1 %
0 - 0.45 %
0 - 0.15 %
This material data has been provided by ASTM.