ASTM A252 Grade 3

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

20 %

Show Material materials with Elongation A50 of 20 %

Tensile strength

23.0 °C

455 MPa

Show Material materials with Tensile strength of 455 MPa

Yield strength

23.0 °C

310 MPa

Show Material materials with Yield strength of 310 MPa

Chemical properties

PropertyValue

Phosphorus

0.04 %

Show Material materials with Phosphorus of 0.04 %