Mechanical

Elongation A

40 % at 20 °C

Tensile strength Rm

373 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

76 - 79 %

Zn

17.81 - 21.98 %

Al

1.8 - 2.5 %

Si

0.2 - 0.5 %

Pb

0.07 %

More

Technological properties

Processing history

annealed