JIS H3300 Grade C7060 O

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A

30 % at 20 °C

Tensile strength Rm

275 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

84.6 - 88.3 %

Ni

9 - 11 %

Fe

1 - 1.8 %

Mn

0.2 - 1 %

Pb

0.06 %

Technological properties

Processing history

annealed

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.