ISO 4954 Grade CC15X UP

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Tensile strength Rm

530 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

0.3 - 0.6 %

C

0.12 - 0.19 %

Al

0 - 0.02 %

P

0 - 0.04 %

Si

0 - 0.1 %

More

Technological properties

Processing history

as rolled ( U ) or as rolled and peeled ( P )

This material data has been provided by MetalInfo.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.