General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 200.0 °C | 188 GPa Show Material materials with Elastic modulus of 188 GPa | |
Hardness, Brinell | 20.0 °C | 240 - 260 [-] Show Material materials with Hardness, Brinell of 240 - 260 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Steel |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K | |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Steel | |
Specific heat capacity | 23.0 °C | 440 - 494 J/(kg·K) Show Material materials with Specific heat capacity of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Thermal conductivity | 100.0 °C | 39.8 W/(m·K) Show Material materials with Thermal conductivity of 39.8 W/(m·K) | |
200.0 °C | 37.7 W/(m·K) Show Material materials with Thermal conductivity of 37.7 W/(m·K) | ||
Chemical properties
Property | Value |
---|---|
Boron | 8E-4 - 5E-3 % Show Material materials with Boron of 8E-4 - 5E-3 % |
Carbon | 0.14 - 0.19 % Show Material materials with Carbon of 0.14 - 0.19 % |
Chromium | 0.8 - 1.1 % Show Material materials with Chromium of 0.8 - 1.1 % |
Manganese | 1 - 1.3 % Show Material materials with Manganese of 1 - 1.3 % |
Phosphorus | 0.03 - 0.04 % Show Material materials with Phosphorus of 0.03 - 0.04 % |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % |
Sulfur | 0.035 % Show Material materials with Sulfur of 0.035 % |