EN 10292 Grade HX220PD +Z, +ZF, +ZA, +AZ, +AS,hot rolled or cold rolled, hot dip coated

.XLSX
.PDF
Save

Description

The steel HX220PD (X=roll condition, P=phosphorus alloyed, D=hot-dip coatable) is producible with the following coatings: - HX220PD+Z (plating Zn) with coating weights (double-sided) of 100, 140, 200, 225 and 275 g/m² (100 g approximate 7,1 µm per side) - HX220PD+ZF (plating Zn-Fe) with coating weights (double-sided) of 100 and 120 g/m² (100 g approximate 7,1 µm per side) - HX220PD+ZA (plating Zn-Al) with coating weights (double-sided) of 095, 130, 185, 200 and 255 g/m² (95 g approximate 7,2 µm per side) - HX220PD+AZ (plating Al-Zn) with coating weights (double-sided) of 100, 150 and 185 g/m² (100 g approximate 13,3 µm per side) - HX220PD+AS (plating Al-Si) with coating weights (double-sided) of 060 and 080 g/m² (100 g approximate 17 µm per side) The hot dip galvanizing refined flat products are available by arrangement on ordering with different coating weights (also per side). Following surface protection types can be delivered: chemical passivated, oiled, chemical passivated and oiled, sealed, phosphated, phosphated and oiled. Mechanical properties are warranted for a period of 3 months for Bake-hardening steels and for a period of 6 months after provision of the products for all other sorts. The same terms are valid for freedom from stretcher strains (surface type B and C). It is suitable for usual welding methods. For higher coating weights on welding are where approppriate necessary special measures. Furthermore suitability for joining by sticking as well as for application of organic coatings. Application: household appliances industry, construction trade, electrical industry, furniture industry, car industry.

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A80, transverse A80,trans

0 - 32 % at 20 °C

Tensile strength, transverse Rm,trans

340 - 400 MPa at 20 °C

Yield strength Rp0.2, transverse Rp0.2,trans

220 - 280 MPa at 20 °C

Thermal

Melting point Tm

1425 °C

Typical for Carbon Steel

Magnetic

Curie temperature Tc

770 °C at 20 °C

Typical for Low Carbon Steel

Chemical properties

Element

Weight %

Comment

Al

0 - 0.02 %

C

0 - 0.06 %

Mn

0 - 0.7 %

P

0 - 0.08 %

Si

0 - 0.5 %

More

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.